Antimony ore benefication processing flowchart and machine

Ore preparation stage

jaw crusher
Crushing and screening
Coarse crushing: jaw crusher crushes the raw ore to <350mm.
Medium and fine crushing: cone crusher or impact crusher further crushes to <50mm.
Screening: vibrating screen classification, control particle size distribution.
Grinding classification

rock gold grinding equipment
Grinding: ball mill or rod mill grinds the ore to -200 mesh, accounting for 60%-80% (adjusted according to the selection requirements).
Classification: spiral classifier or hydrocyclone controls the grinding particle size.
2. Selection process (core link)
Different methods are selected according to the type of ore. Common solutions include:

Solution 1: Single flotation method

SF flotation cell

                                                        Flotation   Machine 
Applicable scenarios: antimony sulfide ore (such as stibnite Sb₂S₃) or arsenic antimony gold ore.
Process:
Rough selection: add collector (such as butyl xanthate, ethyl thiocyanate) and frother (pine oil), and adjust the pH to 4-6.
Concentration/scavenging: Multiple flotation to improve grade and suppress gangue minerals.
Reagent system: Activator (copper sulfate) or inhibitor (water glass) may be required for adjustment.
Option 2: Gravity selection-flotation combined method
Applicable scenarios: Antimony ore with coarse grains or containing coarse grain monomers.
Process:

gold shaking table

                                                     Shaking   Table 

Manganese Jig machine

                                                           Jig  machine 
Gravity selection pre-selection:Jig machine or shaking table tailings to enrich coarse antimony concentrate.
Flotation: Process gravity selection tailings or medium and fine grains to recover fine antimony.
Option 3: Roasting-leaching method
Applicable scenarios: Refractory antimony oxide ore (such as antimony Sb₂O₃) or complex polymetallic ore containing antimony.
Process:
Roasting: Oxidative roasting (500-600℃) converts antimony oxide into soluble antimonate.
Leaching: Leaching with dilute sulfuric acid or sodium chloride solution, and extracting antimony after solid-liquid separation.
Option 4: Hand-selection-gravity selection (small mines)
Applicable scenarios: rich ores or antimony ores with good crystal development.
Process: Manual hand-selection of rich ore blocks, and the remaining ore is re-selected by jigging or shaking table.
3. Dehydration of concentrate and tailings treatment
Dehydration: concentrator + filter (ceramic filter plate or filter press) to reduce the moisture content of concentrate.
Tails treatment: dry stack or filling underground, wastewater is recycled after sedimentation-neutralization treatment.

Send Inquiry