The beneficiation process of tungsten ore can be divided into two main lines based on the type of minerals: gravity separation for wolframite and flotation for scheelite. For complex intergrown ores, a combined process of gravity separation-flotation-magnetic separation is adopted. The core objectives are efficient dissociation, precise separation, low over-grinding, and high recovery rate. The overall process is unified as crushing → grinding and classification → beneficiation → dewatering → wastewater reuse.
1. General basic process (applicable to all ore types): The mainstream three-stage one-closed-circuit crushing and screening process: jaw crushing to <100mm → cone crushing to <20mm → impact/roll crushing to <5mm; vibrating screen classification, >2mm returned for fine crushing, <5mm enters the mill.

JAW CRUSHER

BALL MILL
Low-grade raw ore can be pre-processed using XRT photoelectric separation for pre-enrichment, discarding waste in advance, and improving the grade of ore entering the mill.
Grinding and classification of wolframite: Prioritize rod mill for over-grinding, with one-stage grinding to -200 mesh at 40%-50%; or two-stage closed-circuit grinding (one-stage ball milling + spiral classification, two-stage cyclone), with final -200 mesh at 70%-85%.
Scheelite: Grind to -200 mesh with 80%-85% fineness, ensuring monomer dissociation and strictly controlling over-grinding.
Classification equipment: spiral classifier / hydrocyclone, with unqualified coarse particles returned for regrinding.
Selection operation (core by type): wolframite: primarily relying on gravity separation, with a process consisting of three-stage jigging roughing → four to five-stage table cleaning → middlings regrinding → fine slime recovery.
Scheelite: Mainly flotation, with the process of desulfurization pretreatment → heated flotation (roughing - cleaning - scavenging) → desliming and thickening → dewatering.
Paragenetic ore: mixed flotation → high-intensity magnetic separation → scheelite heating concentration → wolframite gravity separation / flotation.
Dehydration and environmental protection concentrator → disc filter → drying, resulting in low-moisture tungsten concentrate; wastewater is treated mildly/deeply according to gravity separation/flotation, and recycled for reuse.
II. Core Process by Type: Wolframite (Primarily Gravity Separation) Core Logic: Leverage the density difference (7.1-7.5g/cm³) to avoid over-grinding and implement graded feeding.
Key configuration: Multi-stage jigging (coarse particles > 2mm, rapid tailings discarding) + Multi-stage shaking table (fine particles 0.037-2mm, concentrate enrichment) + Middlings regrinding cycle.
Fine slime treatment: Recover with spiral chute/centrifugal concentrator to reduce loss.
The core logic of scheelite (mainly flotation) is that due to the small density difference, gravity separation is ineffective, and flotation relies on surface property differences.
Key steps: Pre-treatment: Remove sulfides by flotation, add dispersant for desliming, and control pH at 8.5-9.5 (adjusted with sodium carbonate).
Flotation reagent: collector using fatty acids (sodium oleate), depressant using water glass/starch, and heating to 40-60℃ to enhance selectivity.
Process: roughing → cleaning → scavenging. White tungstate enters the foam, while gangue remains in the launder.
The mainstream process for processing scheelite-wolframite intergrowths involves the following steps: bulk flotation of sulfide ore → bulk flotation of scheelite and wolframite → temperature-enhanced cleaning of scheelite → high-intensity magnetic separation of scheelite tailings → recovery of wolframite through gravity separation.
Difficulty: Precise separation, taking into account the dissemination characteristics and recovery efficiency of both minerals.
III. Key Process Points and Core Control Indicators for Wolframite: Prevent over-grinding (prefer rod milling), classify and feed, and treat fine slime separately.
Scheelite: fine grinding and dissociation, pre-removal of impurities, heated flotation + reagent optimization.
Industry access indicators for new construction/renovation projects: ore dressing recovery rate ≥82%, comprehensive energy consumption per ton of raw ore ≤1.7kg standard coal; promote energy-saving equipment and automation, and eliminate manual sorting.
Common equipment combinations for crushing include: jaw crusher + cone crusher + impact crusher; for grinding, there are rod mills and ball mills; for classification, there are spiral classifiers and cyclones; for beneficiation, there are jigs, shaking tables, flotation machines, and high-intensity magnetic separators; for dewatering, there are thickeners and disc filters.
IV. Process selection recommendation for wolframite (coarse-grained dissemination): Focus on gravity separation, equipped with 3-stage jig machine + 4-5 stages of table concentration + regrinding of middlings, balancing recovery rate and cost..

Jig Machine

Shaking Table
Scheelite (fine-grained dissemination): Mainly rely on flotation, grind to over 80% passing -200 mesh, apply heated flotation + high-efficiency reagents, and provide supporting desulfurization and desliming processes.

Flotation Machine
Paragenetic ore: Combined process, involving initial bulk flotation followed by separation, integrating high-intensity magnetic separation and gravity concentration to maximize the recovery of two tungsten minerals.