What is the process flow for beneficiating pyrite?

Flotation Machine
Detailed Explanation of Three Core Processes
1. Flotation machine: The Most Mainstream and Effective Method
Flotation is the core technology for separating pyrite, especially suitable for processing fine-grained ores with low grades.
Principle: Utilizing the natural or modified hydrophobicity of the pyrite surface, reagents are added to make it adhere to air bubbles, separating it from waste rock.
Common Reagents:
Collectors: Butyl xanthate, isopropyl xanthate, etc.
Frothers: No. 2 oil (pine oil).
Modifiers: In specific processes, oxalic acid or copper sulfate may be used as activators, or lime as a depressant (used to separate pyrrhotite and pyrite).
Applicable Scenarios: Most pyrite ores, especially when high-grade sulfur concentrate (S > 40%) is required.
2. Gravity Separation: A Low-Cost, Environmentally Friendly Pre-Enrichment Method
For coarse-grained or high-grade pyrite ores, gravity separation can significantly reduce costs.
Equipment: Jig machine (for coarse particles), shaking table (for fine particles).

Jig Machine
Advantages: Requires no chemical reagents, low cost, environmentally friendly, and often used as a pre-enrichment stage before flotation.
Case Study: A carbonaceous pyrite deposit in Guizhou Province can be first gravity-separated using shaking tables to obtain a rough concentrate with a sulfur grade of 28.96% and a recovery rate of 72.19%. Subsequent flotation yields a qualified sulfur concentrate with a final grade of 42.76%.

Shaking Table
3. Magnetic Separation: Primarily used to separate iron and sulfur.
When magnetite or pyrrhotite is associated with pyrite, magnetic separation is a crucial separation method.
Typical Process: A combined "magnetic-flotation-magnetic" process.
Step 1: Weak magnetic separation to recover strongly magnetic iron minerals.
Step 2: Flotation of the magnetic product to remove pyrite (pyrrhotite or pyrite).
Step 3: Second magnetic separation to finally obtain a high-grade iron concentrate.
Results: Using this process, a difficult-to-process ore from Liaoning Province ultimately yielded a qualified iron concentrate with an iron grade of 67.20% and a sulfur content of only 0.36%, and a sulfur concentrate with a sulfur grade of 32.30% was also recovered.
Summary and Recommendations
The choice of process depends on your objectives:
If the primary goal is sulfur recovery, the combined "gravity separation + flotation" process is the best combination, offering the highest cost-effectiveness.
If the ore has higher iron value, a "magnetic-flotation-magnetic" process is needed to increase iron and reduce sulfur.
For small-scale operations or processing coarse waste rock, simple gravity separation (jigging or shaking table) is sufficient and economical.
Recommended beneficiation tests: Regardless of the process chosen, laboratory beneficiation tests on the specific ore are strongly recommended. The particle size distribution and associated relationships (pure pyrite or pyrrhotite) of pyrite from different origins vary greatly, requiring testing to determine the optimal grinding fineness and reagent regime.